Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1515 MPa @Strain 0.200 % |
219700 psi @Strain 0.200 % |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 1515 MPa | 219700 psi | Oil Quenched from 871°C; 427°C Temper Temperature |
Latrobe Staminal™ Shock Resisting Die Steel Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, .. |