Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1240 MPa | 180000 psi | |
Kinetics MIM 440C Stainless Steel Martensitic stainless steel. Excellent strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Often used for automotive, cutlery, industrial equipment, power han.. |
|||
Tensile Strength, Yield | 1240 - 1520 MPa | 180000 - 220000 psi | |
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Tensile Strength, Yield | 1240 - 1520 MPa | 180000 - 220000 psi | |
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Tensile Strength, Yield | 1241 MPa | 180000 psi | |
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide s.. |
|||
Tensile Strength, Yield | 1240 MPa | 180000 psi | ASTM D3039 |
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is id.. |
|||
Tensile Strength, Yield | 1240 MPa | 180000 psi | |
Wingate Alloys Winco-Tuf 50 Ultra High Strength Alloy Wear Plate Winco-Tuf 50 quenched and tempered, high alloy steel is intended specifically for applications requiring a high degree of abrasion and wear resistance.Used by industries such as mining, forestry, qu.. |
|||
Tensile Strength, Yield | 1241 MPa @Strain 0.200 %, Temperature 371 °C |
180000 psi @Strain 0.200 %, Temperature 700 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Tensile Strength, Yield | 1240 MPa @Strain 0.200 % |
180000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Tensile Strength, Yield | 1241 MPa | 180000 psi | |
HP Alloys Alloy 718, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Tensile Strength, Yield | >= 1241 MPa @Strain 0.200 % |
>= 180000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 5 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 1.5 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |
|||
Tensile Strength, Yield | >= 1241 MPa @Strain 0.200 % |
>= 180000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked Level 5 Cold Worked applies to tensile properties of 0.25 to 1.5 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |