Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.8 MPa | 1570 psi | -10% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N75L Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Ultra-Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000/SAE J200 line call-out: MBF710, B34, F19.Application.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1570 psi | ASTM D638 |
Chevron Phillips 1400 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Good Flexibility, Good Flow, Good Warping Resistance, Good Mold Release, Good ESCRApplications:Lids & Closures, C.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1570 psi | 500 mm/min; ASTM D638 |
Eastman 1840A Polyethylene
(discontinued **) Polyethylene 1840A is a low-density formulation with no slip or antiblock. It is suggested for injection molding applications requiring good stiffness, gloss, good processability or layflat properti.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1570 psi | 500 mm/min; ASTM D638 |
Eastman 1840E Polyethylene
(discontinued **) Polyethylene 1840E is a low-density formulation for general extrusion.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer app.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1570 psi | ASTM D412 |
Vicone High Performance Rubber VicoFluro™ 106F-BK High Performance Fluoroelastomer Information provided by Vicone |
|||
Tensile Strength, Yield | 10.8 MPa | 1570 psi | |
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1570 psi | |
Dow Primacor® 4311 Ethylene Acrylic Acid (EAA) PRIMACOR® 4311 polymer containing 3% comonomer 3 is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion to metallic, p.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1570 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3985 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |