Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1070 MPa | 155000 psi | |
Pacific Sintered Materials FN-253-T(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | >= 1070 MPa @Temperature 1025 °C, Time 14400 sec |
>= 155000 psi @Temperature 1877 °F, Time 4.00 hour |
|
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Tensile Strength, Yield | 1070 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
Tensile Strength, Yield | 1070 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
Typical |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4986 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4986.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
Tensile Strength, Yield | 1070 MPa | 155000 psi | Hard |
California Fine Wire Permanickel® K-300 Nickel Alloy All values may vary dependent on specific design and usagePermanickel® is a registered trade name of the Inco family of products.Capabilities: WireRibbonInsulatedPlatedInformation provided by Calif.. |
|||
Tensile Strength, Yield | 1069 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age Data provided by Allvac.Applications: Compressor discs, heavy section forgings for gas turbine engine components. High tensile strength and good fracture toughness. |
|||
Tensile Strength, Yield | 1069 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 15-5 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts. |
|||
Tensile Strength, Yield | 1069 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 17-4 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts. |
|||
Tensile Strength, Yield | 1070 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 400 Thickness >80-100 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Tensile Strength, Yield | 1070 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 400 Thickness 5 - A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Tensile Strength, Yield | 1069 MPa | 155000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 1070 MPa | 155000 psi | Trans. |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Tensile Strength, Yield | 1070 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 400 Thickness 16-80 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Tensile Strength, Yield | 1069 MPa | 155000 psi | |
HP Alloys Alloy 718, 25% Cold Worked 25% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |