Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D412 |
Polymax® Maxelast® P3785 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 1830A Polyethylene
(discontinued **) Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyet.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 1830E Polyethylene
(discontinued **) Polyethylene 1830E is a low density formulation. It is suggested for general purpose extrusion applications, such as tubing and blow molding. Polyethylene 1830E meet the requirements of FDA regula.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | Molded; ASTM D638 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | @50% Elongation; ASTM D1414 |
Greene Tweed FLUORAZ® 790 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D412 |
Teknor Apex APEX® 3300-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D412 |
Teknor Apex APEX® 90-A41R-60-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D412 |
Teknor Apex APEX® 3200-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | |
Dow LDPE 510I Low Density Polyethylene DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | |
Dow Primacor® 4608 Ethylene Acrylic Acid (EAA) PRIMACOR® 4608 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating resin. It is designed to provide excellent adhesion to metallic, paper and polyethylene substrat.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D-638 |
Axiall 59996J Moldings & Extrusions Flexible PVC Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D-638 |
Axiall 8610 Moldings & Extrusions Flexible PVC A high quality, low gravity, clear extrusion and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D-638 |
Bapolene® 2292 Polyethylene Film Grade Bapolene 2292 is a butene linear low density polyethylene copolymer designed to provide a combination of toughness and stiffness and complies with FDA 21 CFR177.1520.Applications: Closures, lids, an.. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D-638 |
Axiall 50896 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 10.7 MPa | 1550 psi | ASTM D-638 |
Axiall 8603 Moldings & Extrusions Flexible PVC A soft extrusion compound with rubber-like properties and oil resistance. Ideally suited for extruded profiles, tubings and co-extruded shapes.Information provided by Georgia GulfGeorgia Gulf becam.. |