Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 970 MPa | 141000 psi | |
Industeel Superplast® 350 Mold Steel SUPERPLAST® 350 offers improved machinability, improved consistency and weldability, improved thermal conductivity, with a higher hardness allowing better mechanical properties and polishability... |
|||
Tensile Strength, Yield | 970 MPa @Strain 0.200 % |
141000 psi @Strain 0.200 % |
|
Haynes 25 alloy, cold worked sheet, 20 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 972 MPa @Strain 0.200 % |
141000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 970 MPa @Strain 0.200 %, Temperature 550 °C |
141000 psi @Strain 0.200 %, Temperature 1020 °F |
Precipitation Hardened prior to test |
Special Metals INCOLOY® Alloy 907 A nickel-iron-cobalt alloy with additions of niobium and titanium for precipitation hardening. It has the low coefficient of expansion and high strength of INCOLOY alloy 903 but with improved notch.. |
|||
Tensile Strength, Yield | 970 MPa @Strain 0.200 % |
141000 psi @Strain 0.200 % |
Typical |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4987 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4987.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
Tensile Strength, Yield | >= 970 MPa @Strain 0.200 % |
>= 141000 psi @Strain 0.200 % |
|
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i.. |
|||
Tensile Strength, Yield | 970 MPa | 141000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Tensile Strength, Yield | 972 MPa | 141000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 60% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 970 MPa @Strain 0.200 % |
141000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 320 Thickness >80-100 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm.. |
|||
Tensile Strength, Yield | 970 MPa @Strain 0.200 % |
141000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 320 Thickness 16-80 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm.. |
|||
Tensile Strength, Yield | 970 MPa @Strain 0.200 % |
141000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 320 Thickness 5 - A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm.. |
|||
Tensile Strength, Yield | 975 MPa | 141000 psi | R<sub>e</sub>. 500°C tempering temperature. Quenching in oil ø 120. Testpiece hardened by oil quenching from 850°C. |
Assab Steels 705M Machinery Steel ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde.. |