Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 130 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.896 MPa
130 psi
at 200%, no post cure- press cured for 5 minutes; ASTM D412
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Yield 0.896 MPa
130 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5401 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 0.896 MPa
130 psi
ASTM D412
Saint-Gobain COHRlastic® R10470 Firm General-Purpose Silicone Sponge Rubber
Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons..
Tensile Strength, Yield 0.896 MPa
130 psi
ASTM D-412
Saint-Gobain Normount® V4600 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive
Description: Ideal for Exterior Mounting Applications: Normount® V2800/V4600 closed-cell foam bonding tapes are highly conformable. The foam substrate allows energy and stress in the joint to be ..
Tensile Strength, Yield 0.896 MPa
130 psi
ASTM D-412
Saint-Gobain T-Bond II® Semi-Rigid Polyurethane Foam Structural Glazing and Cladding Spacer System
Description: Semi-Rigid Polyurethane Foam Substrate used as a Structural Glazing and Cladding Spacer System for In-Shop Fabrication. Semi-Rigid Polyurethane: An open cell structure allows air and mo..
Tensile Strength, Yield 0.896 MPa
130 psi
ASTM D-412
Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive
Description: Ideal for Exterior Mounting Applications: Normount® V2800/V4600 closed-cell foam bonding tapes are highly conformable. The foam substrate allows energy and stress in the joint to be ..
Tensile Strength, Yield 0.896 MPa
130 psi
at 100%; ASTM D412
G-2706 Styrene-based Biomedical Elastomer
Tensile Strength, Yield 0.896 MPa

@Strain 300 %
130 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3730 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding..
Copyright © lookpolymers.com All Rights Reserved