Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.20 MPa | 1190 psi | ASTM D412 |
Polymax® Maxelast® D6870 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Strength, Yield | 8.20 MPa | 1190 psi | ASTM D412 |
Polymax® Maxelast® P3875H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 8.24 MPa | 1190 psi | |
Microcell Composite Company CELLOMER® 3000 SBS Rubber Pellets CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company |
|||
Tensile Strength, Yield | 8.20 MPa | 1190 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 37-031 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Specialty Thermoplastic ElastomerMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |