Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 804 MPa | 117000 psi | at Center, Transverse |
International Mold Steel P20 Plastic Mold Steel P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel.
Information provided by International Mold Steel. |
|||
Tensile Strength, Yield | 810 MPa @Strain 0.200 %, Temperature 425 °C |
117000 psi @Strain 0.200 %, Temperature 797 °F |
|
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 810 MPa @Strain 0.200 % |
117000 psi @Strain 0.200 % |
|
Haynes 625 alloy, plate after 8000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 810 MPa @Strain 0.200 % |
117000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals INCOLOY® Alloy 925 A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista.. |
|||
Tensile Strength, Yield | 806 MPa @Strain 0.200 % |
117000 psi @Strain 0.200 % |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Tensile Strength, Yield | 807 MPa @Strain 0.200 %, Temperature 538 °C |
117000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |