Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.72 MPa | 1120 psi | ASTM D412 |
Polymax® Maxelast® F7870 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Strength, Yield | 7.72 MPa | 1120 psi | ASTM D412 |
Polymax® Maxelast® P3970H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 7.70 MPa | 1120 psi | ASTM D638 |
Chevron Phillips 1008.5 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 14200Characteristics: Excellent Flexibility, Excellent Flow, Good Warping Resistance, Moderate Mold Release, Moderate ESCRApplications:.. |
|||
Tensile Strength, Yield | 7.70 MPa | 1120 psi | Insulating Layer |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Tensile Strength, Yield | 7.73 MPa | 1120 psi | |
Microcell Composite Company CELLAMP® 5000 Pellets CELLAMP® Pellets can be used for producing foaming boards with damping properties, which yield the best efficiency between -10°C and room temperature.Information provided by Microcell Composit.. |
|||
Tensile Strength, Yield | 7.72 MPa | 1120 psi | ASTM D412 |
Teknor Apex Flexalloy® 3501-40-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 7.72 MPa | 1120 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7182B Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 7.70 - 64.8 MPa | 1120 - 9400 psi | Average value: 10.8 MPa Grade Count:138 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |