Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 731 MPa | 106000 psi | |
Kinetics MIM 17-4PH Stainless Steel (As Sintered) Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat.. |
|||
Tensile Strength, Yield | >= 730 MPa @Strain 0.200 %, Diameter 9.52 mm |
>= 106000 psi @Strain 0.200 %, Diameter 0.375 in |
CWSR; DAN 2700.9 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Yield | >= 730 MPa @Diameter 12.7 - 25.4 mm, Strain 0.200 % |
>= 106000 psi @Diameter 0.500 - 1.00 in, Strain 0.200 % |
CWSR; DAN 2700.9 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Yield | 730 MPa @Strain 0.200 % |
106000 psi @Strain 0.200 % |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 731 MPa | 106000 psi | |
HP Alloys Alloy X, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |