Mechanical Properties Metric English Comments
Tensile Strength, Yield 95.0 - 821 MPa
13800 - 119000 psi
Average value: 286 MPa Grade Count:10
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Tensile Strength, Yield 707 - 821 MPa
102000 - 119000 psi
1"x 0.020" Aramid/Glass
Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements
GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and..