Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 552 - 689 MPa @Strain 0.200 % |
80000 - 100000 psi @Strain 0.200 % |
|
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper AT(TF00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Tensile Strength, Yield | 552 - 689 MPa @Strain 0.200 % |
80000 - 100000 psi @Strain 0.200 % |
|
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper AT(TF00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Tensile Strength, Yield | 483 - 689 MPa @Strain 0.200 % |
70000 - 100000 psi @Strain 0.200 % |
Escomatic Coils |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Tensile Strength, Yield | 483 - 689 MPa @Strain 0.200 %, Thickness <=25.4 mm |
70000 - 100000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Tensile Strength, Yield | 483 - 689 MPa @Strain 0.200 % |
70000 - 100000 psi @Strain 0.200 % |
Escomatic Coils |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Tensile Strength, Yield | 483 - 689 MPa @Strain 0.200 %, Thickness <=25.4 mm |
70000 - 100000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Tensile Strength, Yield | 538 - 689 MPa | 78000 - 100000 psi | 0.2% offset |
Eagle Brass 64725 MAX251C, Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Tensile Strength, Yield | 579 - 689 MPa | 84000 - 100000 psi | 0.2% offset |
Eagle Brass 770 Nickel Silver 18%, 3/4 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |