Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.00 - 6.00 MPa @Temperature 120 - 120 °C |
435 - 870 psi @Temperature 248 - 248 °F |
Average value: 4.50 MPa Grade Count:2 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Yield | 3.00 - 6.00 MPa @Temperature 120 °C |
435 - 870 psi @Temperature 248 °F |
ASTM D638 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Tensile Strength, Yield | 3.00 - 6.00 MPa @Temperature 120 °C |
435 - 870 psi @Temperature 248 °F |
ASTM D638 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |