Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 - 30.0 MPa
3630 - 4350 psi
ISO.527 DN.53455
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
Tensile Strength, Yield 25.0 - 30.0 MPa
3630 - 4350 psi
ISO.527 DN.53455
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
Tensile Strength, Yield 20.0 - 30.0 MPa
2900 - 4350 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Tensile Strength, Yield 6.89476 - 30.0 MPa

@Temperature -30.0 - 70.0 °C
1000.00 - 4350 psi

@Temperature -22.0 - 158 °F
Average value: 20.6 MPa Grade Count:1
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Tensile Strength, Yield 20.0 - 30.0 MPa
2900 - 4350 psi
Average value: 27.0 MPa Grade Count:7
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..