Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.0 - 22.8 MPa | 2030 - 3300 psi | Average value: 18.9 MPa Grade Count:18 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Tensile Strength, Yield | 10.0 - 22.8 MPa | 1450 - 3300 psi | Average value: 17.9 MPa Grade Count:45 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |