Polymer Property : Tensile Strength, Yield = 20.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 - REG PE Multicoloured coarse
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, AST
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, Black
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, Conductive
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, MoS2 -Moly-
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 PE-UHMW, UV - stabilized
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 500 - REG PE Colored
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Tensile Strength, Yield 10.0 - 20.0 MPa
1450 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 500 - REG PE Multicoloured coarse
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Tensile Strength, Yield 10.0 - 20.0 MPa
1450 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 500 - REG PE Multicoloured fine
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 500 PE-HMW, AST
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Okulen® 1000 - REG PE Multicoloured fine
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Tensile Strength, Yield 14.0 - 20.0 MPa
2030 - 2900 psi
Average value: 16.6 MPa Grade Count:5
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Tensile Strength, Yield 17.0 - 20.0 MPa
2470 - 2900 psi
ASTM D638M
DSM Somos® 9420 Epoxy Resin for Stereolithography
DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid..