Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 40.0 - 157 MPa | 5800 - 22800 psi | Average value: 111 MPa Grade Count:78 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Tensile Strength, Yield | 110 - 157 MPa | 16000 - 22800 psi | Average value: 139 MPa Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |