Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 9.32 MPa | >= 1350 psi | |
Kazanorgsintez 11503-070 UUP Low Density Polyethylene Production Method: LDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Designed for packaging and production of products designed for food contact, toy p.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | 200 mm/min; ASTM D638 |
LG Chemical LUTENE LB4500 LDPE Extrusion Coating Description: LUTENE LB4500 is mainly intended for extrusion coating and can be processed uniform thickness and width. LUTENE LB4500 is also noted for the excellent heat stability and has good silico.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | ASTM D638 |
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, hous.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S190A Thermoplastic Polyurethane Type: Estane® S190A is a Shore 92A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® X-585A-31 Thermoplastic Polyurethane Type: Estane® X585A-31 is a Shore 95A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizol.. |
|||
Tensile Strength, Yield | 9.32 MPa | 1350 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® CR185A Thermoplastic Polyurethane Type: Estane® CR185A is a Shore 85A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |