Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 896 MPa | 130000 psi | 0.2% offset |
Niagara LaSalle e.t.d.® 150® Cold Finished Steel Bar e.t.d.® 150® is produced from AISI medium carbon 4100 series alloy steel. The heats to be used for e.t.d. 150® are controlled to contain nitrogen in quantities normally associated with steel prod.. |
|||
Tensile Strength, Yield | 896 MPa | 130000 psi | |
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel 9310 VAC-ARC is a premium quality alloy carburizing steel produced by the vacuum consumable electrode process. It has a high hardenability, high core hardness and high fatigue strength, all of which.. |
|||
Tensile Strength, Yield | >= 896 MPa @Strain 0.200 % |
>= 130000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 3 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 2.4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion res.. |
|||
Tensile Strength, Yield | 896 MPa @Temperature 22.0 °C |
130000 psi @Temperature 71.6 °F |
Hardened and tempered to 34 HRC |
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin.. |
|||
Tensile Strength, Yield | 896 MPa @Temperature 22.0 °C |
130000 psi @Temperature 71.6 °F |
Hardened and tempered to 34 HRC |
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du.. |
|||
Tensile Strength, Yield | >= 896 MPa @Strain 0.200 % |
>= 130000 psi @Strain 0.200 % |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 70% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C (1350°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Tensile Strength, Yield | 896 - 965 MPa @Strain 0.200 % |
130000 - 140000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS03 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 896 - 999 MPa @Strain 0.200 % |
130000 - 145000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS04 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum K12® Dual Hardness Steel This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.The comp.. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 %, Temperature 427 °C |
130000 psi @Strain 0.200 %, Temperature 801 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 896 MPa | 130000 psi | |
HP Alloys Alloy 718, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Tensile Strength, Yield | >= 896 MPa @Strain 0.200 % |
>= 130000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 3 Cold Worked Level 3 Cold Worked applies to tensile properties of 0.25 to 2.4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |
|||
Tensile Strength, Yield | 896 MPa @Temperature 177 °C |
130000 psi @Temperature 351 °F |
Offset not given |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |