Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D412 |
Precision Polymer Engineering E70Q Ethylene Propylene Rubber Peroxide cured, Ethylene Propylene Terpolymer, 70-80 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Complies to FDA code of Federal regulations title CFR21 section 177.2600. Water an.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | -20% change after 70 hours @ 125°C; ASTM D412 |
Precision Polymer Engineering E70X Ethylene Propylene Rubber Peroxide cured, Ethylene Propylene Rubber, 65-75 °IRHD. Copolymer of ethylene and propylene.Applications: Excellent water and steam resistance with good compression set properties. Superior heat a.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | -20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering E80B Ethylene Propylene Rubber General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistan.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | -20% change after 70 hours @ 125°C; ASTM D412 |
Precision Polymer Engineering E90K Ethylene Propylene Rubber General purpose, peroxide cured, Ethylene Propylene Terpolymer, 85-95 °IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM D2000/SAE J200 line call out M8CA910, A25, B35, C32, EA14, .. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ISO 527 |
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa. |
|||
Tensile Strength, Yield | >= 8.00 MPa | >= 1160 psi | -20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N70L Nitrile Rubber Nitrile Butadiene Rubber (NBR), 70 °IRHD. Low- Med acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet: ASTM D2000/SAE J200 line call-out: M5BG710, A14, B14, EO14, EO34.. |
|||
Tensile Strength, Yield | 8.00 - 12.0 MPa | 1160 - 1740 psi | ±20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N90K Nitrile Rubber Peroxide cured Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. ASTM D2000/SAE J200 line call-out M7BG910, B14, EA14, EF11, EF21.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | -20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering Q90A Polyurethane Rubber Peroxide cured, blue Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion .. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | -20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering Q90B Polyurethane Rubber Peroxide cured, Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | -20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering Q90Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D412 |
Precision Polymer Engineering S60Z Silicone Rubber Grey Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Fo.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D412 |
Precision Polymer Engineering S70R Silicone Rubber Red Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and lo.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D412 |
Precision Polymer Engineering V75E Fluoroelastomer Compound Special steam resistant, Green Fluoroelastomer Rubber, 71-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F1.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | 20 in/min, injection molded, type 1 specimen; ASTM D638 |
Phillips Sumika Marlex® CHP-010 Thermoplastic Polyolefin
(discontinued **) Applications: Soft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D638 |
Huntsman PE5082 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D638 |
Huntsman PE1651 EVA Film Extrusion
(discontinued **) 6.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with outstanding low temperature strength, excellent clarity, and good heat seal.Applications: Film extrusion: ice bags, liqui.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICOTEXâ„¢ 520-5019 300 Micron LDPE Powder Description: ICOTEX 520-5019 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ISO 527/2 |
Iran Petrochemical (PCC) 1922T Low Density Polyethylene LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3211-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | ASTM D412 |
Teknor Apex APEX® 3211-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | |
Trelleborg B571 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | |
Trelleborg Hypalon® H711 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | |
Trelleborg S850 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | |
Trelleborg T620 Butyl Rubber Butyl rubber is a copolymer of isobutylene and a small percentage of isoprene.PropertiesWith careful compounding Butyl has really good tensile strength.Butyl has very low permeability to air and oth.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | |
Trelleborg E350 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | 8.00 MPa @Strain 50.0 % |
1160 psi @Strain 50.0 % |
|
Covestro Texin® 950 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated f.. |
|||
Tensile Strength, Yield | 8.00 MPa | 1160 psi | 50 mm/min |
Arkema Group Evatane® 1005 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent film with high strength, shrinking at low temperature. Examples: curtain stretch, coextrusion, .. |