Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 790 - 940 MPa | 115000 - 136000 psi | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM04 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 77%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | >= 790 MPa | >= 115000 psi | |
MetalTek MTEK CA20NW Cast UNS J91631 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 790 - 1040 MPa | 115000 - 151000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 790 - 1040 MPa | 115000 - 151000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 790 MPa @Strain 0.200 %, Temperature 540 °C |
115000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 790 MPa @Strain 0.200 % |
115000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals MONEL® Alloy K-500 A precipitation-hardenable nickel-copper alloy that combines the corrosion resistance of MONEL alloy 400 with greater strength and hardness. It also has low permeability and is nonmagnetic to under.. |
|||
Tensile Strength, Yield | >= 790 MPa | >= 115000 psi | |
MetalTek MTEK H46 Martensitic Stainless Steel "400" series, General corrosion resistant alloy, high strength.Applications: Chemical and food process equipment, jet engine compressor cases and rocket engine parts.Information provided by MetalTek.. |