Mechanical Properties Metric English Comments
Tensile Strength, Yield 676 MPa

@Temperature 23.9 °C
98000 psi

@Temperature 75.0 °F
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D638
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Tensile Strength, Yield 676 MPa

@Temperature 21.1 °C
98000 psi

@Temperature 70.0 °F
0° Direction, Dry; Autoclave Cured; ASTM D3039-95
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 34-700 12K 2x2 Twill Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Tensile Strength, Yield 676 MPa
98000 psi
Meehanite K-295 Austempered Ductile Iron
Type K-295 is used for applications such as gears requiring high contact rolling and tooth bending fatigue properties. Type K-295 also possess high fracture toughness impact strength. Excellent fo..
Tensile Strength, Yield 676 - 758 MPa
98000 - 110000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 676 MPa

@Strain 0.200 %
98000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..
Copyright © lookpolymers.com All Rights Reserved