Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.16 MPa

@Temperature 23.0 °C
893 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE)
Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough..