Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.24 - 6.31 MPa
760 - 915 psi
Average value: 5.69 MPa Grade Count:3
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Tensile Strength, Yield 5.24 MPa

@Strain 300 %
760 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Synprene® RT-5180 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength, Yield 5.24 MPa
760 psi
at 200%, no post cure- press cured for 5 minutes; ASTM D412
Multibase C6-570 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 5.24 MPa
760 psi
100%; ASTM D412
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Tensile Strength, Yield 5.24 MPa
760 psi
ASTM D638
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin
Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A..