Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 485 MPa | >= 70300 psi | |
MetalTek MTEK 420 Cast UNS J91153 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
|
Haynes 188 alloy, plate at RT after 0 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
|
Haynes 230® alloy, 30% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Tensile Strength, Yield | >= 485 MPa | >= 70300 psi | |
MetalTek MTEK 29M Cast UNS J93370 Duplex Stainless Steel Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels.Applications: Offshore piping systems, couplings. Centrifuge, dewatering equipment. Pump, v.. |
|||
Tensile Strength, Yield | >= 485 MPa | >= 70300 psi | |
MetalTek MTEK 29MN Cast UNS J93372 Duplex Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature sheet after 500 hours of 650°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
|
Haynes 556® alloy, 50% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
|
Haynes 625 alloy, 20% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 485 MPa | 70300 psi | |
ATI Allegheny Ludlum AL 625HP™ Stainless Steel Nickel-based superalloy. Characteristics:exceptional fatigue resistance, excellent resistance to oxidation and corrosion, outstanding strength and toughness over a range of temperatures from cryogen.. |
|||
Tensile Strength, Yield | 485 - 515 MPa | 70300 - 74700 psi | T direction |
ArcelorMittal Speed 35-440 Electrical Steel Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
|
ATI Allvac® REX 734™ UNS S31675 Specialty Steel Uses: Medical and surgical devices; forged mono-block hip stems.Property values are for samples in the metallurgical condition: As rolled, warm worked.Information provided by Allvac, An Allegheny Te.. |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AM 350™ High Strength Specialty Steel Alloy, UNS S35000 Property data below is typical of annealed samples. Available in sheet and strip only. For use in valves, aircraft tubing, bellows, mounts, brackets, and ducts.Information provided by Allegheny Lu.. |