Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 462 MPa @Strain 0.200 % |
67000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 462 MPa @Strain 0.200 % |
67000 psi @Strain 0.200 % |
|
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 10% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of t.. |
|||
Tensile Strength, Yield | 462 - 510 MPa | 67000 - 74000 psi | 0.2% offset |
Eagle Brass 194 HSM® Copper, Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Yield | 462 - 510 MPa | 67000 - 74000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, Extra Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Yield | 462 - 538 MPa | 67000 - 78000 psi | 0.2% offset |
Eagle Brass 260 Cartridge Brass, Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Yield | 462 - 552 MPa | 67000 - 80000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 462 - 572 MPa | 67000 - 83000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, 3/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Yield | 462 - 538 MPa | 67000 - 78000 psi | 0.2% offset |
Eagle Brass 735 Nickel Silver 18%, Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 462 MPa @Strain 0.200 %, Temperature -129 °C |
67000 psi @Strain 0.200 %, Temperature -200 °F |
Transverse |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 462 MPa @Strain 0.200 %, Temperature 566 °C |
67000 psi @Strain 0.200 %, Temperature 1050 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 462 MPa @Strain 0.200 % |
67000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |