Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 455 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 455 MPa
66000 psi
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 188/ Multimet alloy 12.7 mm plate weldments
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 455 MPa
66000 psi
Mueller Dynalloy Alloy 6730 Free cutting bearing bronze (UNS C67300)
Free cutting bearing bronzeApplications: Dynalloy is widely used for bearing applications, bushings, gears, valve guides, shaft and cylinder guides. The alloy has found wide acceptance in speed red..
Tensile Strength, Yield 455 MPa

@Strain 0.200 %
66000 psi

@Strain 0.200 %
Haynes 556® alloy, 30% cold reduction, 1065°C anneal for 5 minutes
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 455 MPa

@Strain 0.200 %
66000 psi

@Strain 0.200 %
Haynes 625 alloy, plate, as annealed at 1025°C, rapid cooled
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 455 MPa

@Strain 0.200 %
66000 psi

@Strain 0.200 %
As-Consolidated; At Room Temperature
Crucible Compaction Metals P/M N625 Corrosion Resistant Alloy
P/M N625 (chemically, UNS N06625) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The a..
Tensile Strength, Yield 455 MPa

@Temperature 93.0 °C
66000 psi

@Temperature 199 °F
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel
Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s..
Copyright © lookpolymers.com All Rights Reserved