Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 427 MPa @Temperature 23.9 °C |
62000 psi @Temperature 75.0 °F |
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D638 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Tensile Strength, Yield | 427 MPa @Strain 0.200 % |
62000 psi @Strain 0.200 % |
|
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Round Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Round samples. Other property values are typical of INCONEL® alloy 725.Data provided.. |
|||
Tensile Strength, Yield | 427 - 469 MPa | 62000 - 68000 psi | 0.2% offset |
Eagle Brass 151 ZHC® COPPER, Spring Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Yield | >= 427 MPa | >= 62000 psi | 0.2% offset |
Eagle Brass 19210 XP-10 Copper Iron, Spring 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Yield | 427 MPa @Strain 0.200 % |
62000 psi @Strain 0.200 % |
|
Crucible Steel 440B Chromium Steel Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me.. |
|||
Tensile Strength, Yield | 427 MPa @Strain 0.200 % |
61900 psi @Strain 0.200 % |
Annealed |
ATI Allegheny Ludlum 440A Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 427 MPa @Temperature 149 °C |
61900 psi @Temperature 300 °F |
|
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |
|||
Tensile Strength, Yield | 427 MPa | 62000 psi | |
Performance Alloys MoldStar® 22 (PAS 22) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Ejector SleevesLifter BladesThin Wall Appli.. |
|||
Tensile Strength, Yield | 427 MPa @Strain 0.200 % |
61900 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |