Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 40.4 MPa | 5860 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 86110 white 1275 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |