Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 340 - 520 MPa | 49300 - 75400 psi | |
Materion Beryllium Copper Alloy 10 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 340 - 520 MPa | 49300 - 75400 psi | |
Materion Beryllium Copper Alloy 3 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
MetalTek MTEK 825 Cast UNS N08826 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 340 MPa @Strain 0.200 % |
49300 psi @Strain 0.200 % |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Yield | 340 MPa @Strain 0.200 % |
49300 psi @Strain 0.200 % |
Solution Annealed. Value at room temperature |
Special Metals INCONEL® Alloy 617 A nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of metallurgical stability, strength, and oxidation resistance at high temperatures. Resistance to oxidation is enhanced by.. |
|||
Tensile Strength, Yield | 340 MPa @Strain 0.200 % |
49300 psi @Strain 0.200 % |
Annealed prior to test |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 1011, Grade 50 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 607 Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 715 Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel CL 1/ SAE J1392 045 XLK, Grade 50 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel CL 2/ SAE J1392 045 XLK, Grade 50 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel SAE J1392 050 XLK, Grade 50 Aluminized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ZINCGRIP® Class 2, Grade 50 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 20-15 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 25-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 27-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 30-17 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 30-18 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 1011, Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel ASTM A 570, Grade 50 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | >= 340 MPa | >= 49300 psi | |
AK Steel SAE J1392, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel |
|||
Tensile Strength, Yield | 340 MPa | 49300 psi | R<sub>p</sub>02. 200 HB. |
Assab Steels 760 Machinery Steel ASSAB 760 is an easily machinable carbon steel characterized by: Good machinabilityGood mechanical strengthASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be .. |
|||
Tensile Strength, Yield | 340 - 400 MPa | 49300 - 58000 psi | |
ArcelorMittal HSLA 340 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC340LA), electroglavanized (HC340LA +ZE) and Extragal®/galfan/Galvannealed (HC340LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |
|||
Tensile Strength, Yield | 340 MPa @Strain 0.200 % |
49300 psi @Strain 0.200 % |
|
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Tensile Strength, Yield | 340 - 520 MPa | 49300 - 75400 psi | |
Materion Beryllium Copper Alloy 3 Tube; H (TD04) Temper; up to 76 mm o.d. (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |