Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 34.6 MPa | 5020 psi | ASTM D638 |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Tensile Strength, Yield | 34.6 MPa | 5020 psi | ASTM D 638 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |