Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 32.4 MPa | 4700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPH-40T Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ STFPP.1220 BK-L Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2 in per min, tangent; ASTM D638 |
Network Polymers NPP 20-1202 Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 30-1800 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 30-3000 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Petromont 3000 High Density Polyethylene Resin Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and o.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Rochling Engineered Plastics Polystone® P Polypropylene Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Total 620 Polystyrene
(discontinued **) Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high .. |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
PolyMirae Moplen EP332C Pipe Extrusion Grade Polypropylene Moplen EP332C is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP332C is a block copolymer appreciated by customers in the mar.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Flint Hills 23H2A Random Copolymer Polypropylene Features: Excellent clarity. Product does not contain animal derived components.Applications: Designed for Blow molding and Thermoforming - A replacement for PET, PS and PC high clarity applicatio.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
Hyosung Topilene HJ541CP PP HJ541CP High Isostatic PP Impact CopolymerApplications:Cap of pressure bottleCharacteristics:High stiffnessSlip propertyMedium impactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
Hyosung Topilene HJ640A PP HJ640A Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 32.4 MPa @Thickness 3.20 mm |
4690 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 32.4 MPa @Thickness 3.20 mm |
4690 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
Global J-2208 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D 638 |
LyondellBasell Pro-faxâ„¢ SC204 Polypropylene Copolymer Description: Pro-faxâ„¢ SC204 polypropylene copolymer resin is designed for thermoforming and sheet extrusion applications. It is nucleated and features antistatic properties. Pro-faxâ„¢ SC20.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Washington Penn High Modulus Polypropylene Copolymer 15% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 3312E Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3312E is a clarified, medium flow random copolymer with fast cycle time and easy mold release. It is designed for injection .. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 330ºF Cure Temperature MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | at 300%; ASTM D412 |
Lubrizol Estane® ALR PC60D Thermoplastic Polyurethane Type: Estane® ALR PC60D is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableInformation Provided by The Lubrizol Corporation |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
Cheng Yu Plastic PP229H TALC 20 Polypropylene, 20% Talc, High Heat |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | chs 2.0 in/min; tangent; ASTM D638 |
Diamond Polymers NPP30-3500G Homopolymer Polypropylene Granules Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
ExxonMobil Paxon™ AD60-007 Blow Molding Resin Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Amco PRIMATOP HDPE RP 004 Granular High Density Polyethylene HDPE RP 004 features small particle size and is used in plastic lumber extrusion.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP CO 002-12 RC Clarified Random Copolymer Features:low flowcontainers clarifiersexcellent processingexcellent clarityApplications:bottlescontainersFormer A-Top Polymers product; part of Amco product line since 2013. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D-638 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S375D Thermoplastic Polyurethane Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |