Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.79 MPa | 550 psi | at 200%, no post cure- press cured for 5 minutes; ASTM D412 |
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | ASTM D412 |
Polymax® Maxelast® A9855A TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 3.79 - 4.78 MPa | 549 - 693 psi | Flatwise (sandwich); Bag Surface |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | at 100%; ASTM D412 |
MF-5057 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® RP 6568 C Natural TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | @100% Elongation; ASTM D1414 |
Greene Tweed Xyfluor® 870 Fluorinated Elastomer Compound Xyfluor® 870, a highly fluorinated elastomer compound, provides excellent chemical compatibility over a wide range of temperatures from -76°F to 450°F (-60°C to 232°C). Recommended f.. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | Elastic; ASTM D638 |
Multibase Multi-Flex® A 6221 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsAutomotive Under the HoodInfo.. |
|||
Tensile Strength, Yield | >= 3.79 MPa | >= 550 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7182X Fluorocarbon-Elastomer Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3500-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 9100-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3301-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412 |
Teknor Apex UNIPRENE® 7400-40D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412 |
Teknor Apex UNIPRENE® 7400-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | ASTM D638 |
Dow AMPLIFY™ EA 100 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 100 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Tensile Strength, Yield | 3.79 MPa | 550 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 2504LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodFoamableHardness, LowHeat StabilizedOzone ResistantProcessability, Good.. |
|||
Tensile Strength, Yield | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3860MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-4060 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma.. |
|||
Tensile Strength, Yield | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® ST-6160 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs.. |