Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.65 MPa | 529 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GT5200-0002 Black Polypropylene Alloy (PP Alloy) Information provided by PolyOne |
|||
Tensile Strength, Yield | 3.65 MPa | 530 psi | at 100%; ASTM D412 |
1074A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 3.65 MPa | 530 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 504 Perfluoroelastomer Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatur.. |
|||
Tensile Strength, Yield | 3.65 MPa @Strain 300 % |
530 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 38-046E Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:FDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A thermoplastic.. |