Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.17 MPa | 460 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4550 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.17 MPa | 460 psi | ASTM D412 |
Polymax® Maxelast® P1750 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 3.17 MPa | 460 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3500-50 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 3.17 MPa | 460 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-50-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 3.17 MPa @Strain 100 % |
460 psi @Strain 100 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 62-002 BLACK 2001 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications: Multi-PurposeProcessing Method: Injection MoldingInformation provided by PolyOne Corporation |
|||
Tensile Strength, Yield | 3.17 MPa | 460 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3820M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:FDA (Food Contact)Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A thermoplasti.. |
|||
Tensile Strength, Yield | 3.17 MPa @Strain 300 % |
460 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3840E Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A ther.. |
|||
Tensile Strength, Yield | 3.17 MPa | 460 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® ST-6120 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne .. |