Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 29.3 MPa | 4250 psi | ASTM D638 |
Omni Plastics OmniTuff™ CPP TF30 Copolymer Polypropylene Talc Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CR350CS-01 Polypropylene Random Copolymer COPYLENE® CR350CS-01 is a clarified, reactor grade, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release for larger ar.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | aged 96 hours at 158ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 50 mm/min; ASTM D638 |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | ASTM D638 |
Ineos R55C-00 Clarified Polypropylene Copolymer Grade R55C-00 is a high melt flow rate clarified and antistatic random polypropylene copolymer. It is designed for high speed injection molding of thin walled parts requiring very good mold filling .. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 2 in/min; ASTM D638 |
Ineos R05C-00 Polypropylene Random Copolymer Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 2"/min; ASTM D638 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 70% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 2"/min; ASTM D638 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 2"/min; ASTM D638 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 2"/min; ASTM D638 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 70% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 2"/min; ASTM D638 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | aged 96 hours at 158ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | 2"/min; ASTM D638 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | ASTM D638 |
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | ASTM D638 |
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Tensile Strength, Yield | 29.3 MPa | 4250 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |