Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.37 MPa | 3825 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Tensile Strength, Yield | 26.37 MPa | 3825 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Tensile Strength, Yield | 26.37 MPa | 3825 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Tensile Strength, Yield | 26.37 MPa | 3825 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Tensile Strength, Yield | 26.37 MPa | 3825 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Tensile Strength, Yield | 26.37 MPa | 3825 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Tensile Strength, Yield | 26.37 MPa | 3825 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 26.37 MPa | 3825 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |