Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.20 MPa | 3800 psi | ASTM D638 |
ExxonMobil HD 6704.18 Injection Molding Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |