Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.7 MPa | 3580 psi | ASTM D638 |
Multibase Multi-Pro® 2516 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult.. |
|||
Tensile Strength, Yield | 24.7 MPa | 3580 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 7000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 24.7 MPa | 3580 psi | ASTM D638 |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Tensile Strength, Yield | 24.7 MPa | 3580 psi | ASTM D638 |
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 53600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Housewares.. |
|||
Tensile Strength, Yield | 24.7 MPa | 3580 psi | ISO 527-2/50 |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |
|||
Tensile Strength, Yield | 24.7 MPa | 3580 psi | 2 in/min; ASTM D638 |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Tensile Strength, Yield | 24.7 MPa | 3580 psi | ASTM D412 |
Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |