Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.6 MPa | 3420 psi | 50 mm/min; ASTM D638 |
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che.. |
|||
Tensile Strength, Yield | 23.6 MPa | 3430 psi | ASTM D638 |
Ineos N10N-00 Polypropylene Impact Copolymer Grade N10N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and .. |
|||
Tensile Strength, Yield | 23.6 MPa | 3430 psi | ASTM D638 |
Ineos N12N-00 Polypropylene Impact Copolymer Grade N12N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and .. |