Tensile Strength, Yield 21.6 MPa
3130 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable MAF110A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength, Yield 21.6 MPa
3130 psi
ASTM D638
PolyMirae Moplen RP210R Extrusion Coating and Lamination Grade Polypropylene
Moplen RP210R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP210R is a copolymer particularly suitable for extrusion coating and..
Tensile Strength, Yield 21.6 - 23.5 MPa
3130 - 3410 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 21.6 - 23.5 MPa
3130 - 3410 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 21.6 MPa
3130 psi
ASTM D638
I. Stern HIPS SH03 High Impact Polystyrene
Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc.
Tensile Strength, Yield 21.6 MPa
3130 psi
50 mm/min; ASTM D638
LG Chemical SEETEC PH150 HDPE Blown Film Grade
Features: Characteristics : Excellent weather resistance & Environmental stress cracking resistanceAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 20..
Tensile Strength, Yield 21.6 MPa

@Thickness 3.20 mm
3130 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOL HM5302W PP+MF30%, High Impact
Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
Tensile Strength, Yield 21.6 MPa
3130 psi
ISO 527-2
Styron DGF080.00 ESU Polypropylene
Overview: 10% glass filled polypropyleneNaturalMedium flowHeat ResistantInformation provided by Styron
Tensile Strength, Yield 21.6 MPa
3130 psi
at 100% elongation; ASTM D412
Lubrizol Estane® S160D Thermoplastic Polyurethane
Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Tensile Strength, Yield 21.6 MPa
3130 psi
at 100% elongation; ASTM D412
Lubrizol Estane® S360D Thermoplastic Polyurethane
Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
Tensile Strength, Yield 21.6 MPa
3130 psi
2" (50mm) per min.; ASTM D638
Formosa Plastics Formolene® 2575N injection Molded Polypropylene
Impact Copolymer for High Speed injection Molded ApplicationsFormolene® 2575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging, ..
Tensile Strength, Yield 21.6 MPa
3130 psi
ASTM D638
Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative)
Carbon-powder filled, self-lubricating, moisture-repellent material with resistivity levels in the 10^5-10^9 range. This material has the highest impact strength, is lightweight, has excellent abra..
Tensile Strength, Yield 21.6 MPa
3130 psi
Zylog Hipolyene® 3080 HC RM Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Tensile Strength, Yield 21.6 MPa
3130 psi
Zylog Hipolyene® 5131 SX-5 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Tensile Strength, Yield 21.6 MPa
3130 psi
Zylog Hipolyene® 8021 T Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.