Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.83 MPa

@Strain 300 %
410 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Synprene® RT-3770 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength, Yield 2.83 MPa
410 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® E38 Perfluoroelastomer
Chemraz® E38 was specifically developed for high-density plasma systems and diffusion processes where seal reliability and very minimal contamination are essential. The material provides excelle..
Tensile Strength, Yield 2.83 MPa
410 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-150 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 2.83 MPa
410 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7345 Highly Saturated Nitrile Rubber
HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.83 MPa
410 psi
100%; ASTM D412
Teknor Apex APEX® 1519-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company
Tensile Strength, Yield 2.83 MPa

@Strain 300 %
410 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 37-033 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A therm..
Copyright © lookpolymers.com All Rights Reserved