Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.69 MPa | 390 psi | at 200%, as molded |
Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.69 MPa | 390 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-150 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.69 MPa | 390 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.69 MPa | 390 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.69 MPa | 390 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.69 MPa | 390 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3210-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 2.69 MPa | 390 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3211-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 2.69 MPa | 390 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-45-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |