Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.55 MPa
370 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 618 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
Tensile Strength, Yield 2.55 MPa
370 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield >= 2.55 MPa
>= 370 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7336 Highly Saturated Nitrile Rubber
HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.55 MPa
370 psi
100%; ASTM D412
Teknor Apex APEX® 3055-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength, Yield 2.55 MPa
370 psi
100%; ASTM D412
Teknor Apex APEX® 3200-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 2.55 MPa
370 psi
100%; ASTM D412
Teknor Apex Flexalloy® 3500-45 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
Tensile Strength, Yield 2.55 MPa
370 psi
100%; ASTM D412
Teknor Apex Flexalloy® 9100-45 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Tensile Strength, Yield 2.55 MPa
370 psi
100%; ASTM D412
Teknor Apex APEX® 3300-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me..
Tensile Strength, Yield 2.55 MPa
370 psi
at 100% elongation; ASTM D412
Lubrizol Estane® T365A Thermoplastic Polyurethane
Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..
Tensile Strength, Yield 2.55 MPa
370 psi
at 300% elongation; ASTM D412
Lubrizol Estane® T460AH Thermoplastic Polyurethane
Type: Estane® T460AH is a Shore 60A, polyester grade, plasticizer-free, with low hardness and Hydrolytic Stabilizer thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: Americas, ..
Tensile Strength, Yield 2.55 MPa
370 psi
at 100% elongation; ASTM D412
Lubrizol Estane® T465A Thermoplastic Polyurethane
Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..
Tensile Strength, Yield 2.55 MPa

@Strain 300 %
370 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3830E Thermoplastic Elastomer - SBC  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength, Yield 2.55 MPa

@Strain 300 %
370 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 38-082 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerOver-Molding GradeTransparentMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided b..
Tensile Strength, Yield 2.55 MPa
370 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3620 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tensile Strength, Yield 2.55 MPa

@Strain 300 %
370 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-4050 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionPolyOne..
Copyright © lookpolymers.com All Rights Reserved