Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.8 MPa | 2730 psi | ASTM D638 |
NOVA Chemicals Sclair® 8406 BK, 8406 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 18.8 MPa | 2730 psi | ASTM D638 |
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 18.8 - 290 MPa | 2730 - 42100 psi | Average value: 155 MPa Grade Count:251 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Tensile Strength, Yield | 18.8 MPa | 2720 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 18.8 MPa | 2730 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 HR HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Hydrolysis Resistant Appearance: .. |
|||
Tensile Strength, Yield | 18.8 MPa | 2730 psi | 2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897. |
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: XK41 is an extrusion grade of K-Resin SB copolymer designed specifically for improved performance in blends with general purpose polystyrene. It is eas.. |