Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1320 MPa @Strain 0.200 %, Temperature 595 °C |
191000 psi @Strain 0.200 %, Temperature 1100 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 1320 MPa | 191500 psi | |
Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate For extreme abrasion and moderate impact.Winco-Tuf 40 has excellent toughness at high hardness and in heavy sections. For severe impact and abrasions.Advantages: Maximum resistance to abrasion and i.. |