Polymer Property : Tensile Strength, Yield = 1105 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1105 MPa

@Strain 0.200 %
160300 psi

@Strain 0.200 %
Haynes 230® alloy, 30% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 1105 MPa

@Strain 0.200 %
160300 psi

@Strain 0.200 %
Typical
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged
Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET.