Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.03 MPa | 149 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | TM R050-36 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Tensile Strength, Yield | 1.03 - 2900 MPa | 150 - 420000 psi | Average value: 576 MPa Grade Count:102 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | >= 1.03 MPa | >= 149 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7282 Neoprene / Chloroprene UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | Transverse/Width |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.006" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | Transverse/Width |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.008" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | Transverse/Width |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.010" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Tensile Strength, Yield | 1.03 MPa @Strain 300 % |
150 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1107 Thermoplastic Elastomer Notes: General Purpose; OpaqueInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 1.03 MPa @Strain 300 % |
150 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1736R Thermoplastic Elastomer Notes: Soft Material; Overmold onto PP handlesInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | at 150% elongation, maximum |
Dow Corning SILASTIC® 94-595-HC SILICONE RUBBER PART A&B 30 Durometer, 2-part, 1 to 1 mix, translucent, Injection Moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | |
Resinlab® UR3005 Two Part Urethane Elastomer Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen.. |
|||
Tensile Strength, Yield | 1.03 MPa | 150 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 5861 Fluoro-silicone Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc. |