Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.800 MPa | 116 psi | 150°C for 1,000 hrs; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Tensile Strength, Yield | 0.800 MPa | 116 psi | JIS-K-6251(#2)/ASTM D-412 |
Fujipoly Industries Sarcon® GR-Fk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Tensile Strength, Yield | 0.800 MPa | 116 psi | JIS-K-6251(#2)/ASTM D-412 |
Fujipoly Industries Sarcon® GR-HFk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Tensile Strength, Yield | 0.800 MPa | 116 psi | 125°C for 1,000 hrs; JIS-K-6251(#2); ASTM D412 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Tensile Strength, Yield | 0.800 MPa | 116 psi | -40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6251(#2); ASTM D412 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |